As ultra-high-strength low-alloy steel,36NiCrMo16 steel contains 1.8% Cr and 4% Ni elements as strengthening alloy elements as per EN10083 and EN10250 standard.

36NiCrMo16 steel has excellent hardenability due to its high nickel content and appropriate amount of chromium and molybdenum, and parts of general size can be hardened in air.In the quenched and tempered state, it has excellent strength, plasticity and toughness.

36NiCrMo16 steel is often used to make parts that require high strength, torsion and impact resistance, such as machine drive shafts, crankshafts, gears, worms, connecting rods, bolts, nuts, fasteners, etc.

36NiCrMo16 steel has a good set of properties that makes it a suitable material to create various products and parts.

It can be used in various applications:

  • Aviation and aerospace industries
  • Heavy-duty machine parts
  • Large cross-sections
  • Shafts
  • Axles
  • Levers
  • Rocker arms
  • Connecting rods

36NiCrMo16 Steel Mechanical Properties

  • Tensile strength, Rm: 880 - 1180 MPa
  • Yield point, Re: > 685 MPa
  • Elongation, A: 14%
  • Notch toughness, KCU: 35 - 40 J
  • Hardness in softened state < 260 HB
Products parameters

36NiCrMo16 Steel Equivalent Grades 

EU/EN DIN France/AFNOR England/BS
36NiCrMo16 1.6773 35CND16 835M30

      

36NiCrMo16 Chemical Composition 

C Si Mn Cr Mo Ni P S
0.32-0.39 Max 0.4 0.5-0.8 1.6-2.0 0.25-0.45 3.6-4.1 Max 0.025 Max 0.025

36NiCrMo16 Alloy Steel Heat treatment
Soft Annealing: Heat to 650-680°C, cool slowly. This will produce a maximum Brinell hardness of 269.
Normalizing:Temperature: 850-880°C.
Hardening: Harden from a temperature of 835-865°C, 855-885°C followed by oil or quenching.

36NiCrMo16 STEEL FORGING

Initial Forging Temperature:1200-1220℃

Final Forging Temperature:850℃

Heating Rate:Strictly control the heating speed, which should be uniform and stable to prevent cracking caused by improper heating.

Holding Time:Ensure that the material is fully and evenly heated,and the holding time should not be too long or too short.

Forging Ratio:Above 4:1

Post-Forging Treatment:36NiCrMo16 steel is highly sensitive to white spots, and should be in the furnace for dehydrogenation treatment in time after forging.

Product Picture

32NiCrMo12-5

Our factory
product-600-600

Steel Making

product-600-600

Ingot Production

product-750-750

Forged Bars

product-600-600

Machinary

Packing & Delivery

 

pACKING OF STAINLESS STEEL

Packing & Delivery

Packing detail: Spray paint in Bundle or as per client demands. Port:Any Chinese Port
  • The inner size of container is below:

    -- 20ft GP: 5.8m(length) x 2.13m(width) x 2.18m(high)

    -- 40ft GP: 11.8m(length) x 2.13m(width) x 2.18m(high)
    -- 40ft HG: 11.8m(length) x 2.13m(width) x 2.72m(high)

 

 

Our Service

1. Competitive price and quality from our own factory .
2. Best service with 24 hour`s reply .
3. Flexible payment with T/T,L/C , etc .
4. Smooth production ability(1000tons/month).
5. Quick delivery and standard exporting package.



 
product-950-408
 
 

 

Baj popilè: 36nicrmo16 equivalent alloy steel bars, China 36nicrmo16 equivalent alloy steel bars manufacturers, suppliers, factory

Voye rechèch

whatsapp

Telefòn

Mel

Rechèch