18CrNiMo7-6 Alloy Steel Bar
Kapasite chalè espesifik J/(kg.K): 460
Rezistivite elektrik Ohm.mm2 /m: 0.18
Konduktivite elektrik Siemens.m/mm2: 5.55
DIN1.6587/18CrNiMo7-6 se yon kabòn ki ba, ka redi (karburize) asye ki gen 1.8 pousan chromium - nikèl - molybdène kòm ajan ranfòse dapre EN 10084. Karakterize pa gwo fòs nwayo ak severite nan mwayen ak gwo seksyon. ak ka dite jiska Rc62 lè karburize, fè tèt di ak tanperaman, epi li se tou yo itilize nan zòn nan pati lou ak gwo tansyon Kovèti pou ak gwo demand sou severite nan rupture nwayo nan 1050-1350N / mm2.DIN1.6587 / 18CrNiMo{{14 }} se menm jan ak 17CrNiMo6 asye, jeneralman apwovizyone nan kondisyon an rkwit ak yon dite brinell maksimòm de 229
Estanda | Klas | C | Mn | P | S | sizo | Ni | Kr | Mouvman |
EN 10084 | 18CrNiMo7-6 | 0.15-0.21 | 0.50-0.90 | Mwens pase oswa egal a 0.025 | Mwens pase oswa egal a 0.035 | Mwens pase oswa egal a 0.04 | 1.4-1.7 | 1.5-1.8 | 0.25-0.35 |
1.6587 |
Konpozisyon chimik
Dansite, g/cm3 | 7.85 | ||||
Kapasite chalè espesifik J/(kg.K) | 460 | ||||
Rezistivite elektrik Ohm.mm2 /m | 0.18 | ||||
Elektrik konduktivite Siemens.m/mm2 | 5.55 | ||||
Modil Elastisite Gpa | 210 | ||||
Ekspansyon tèmik 10^6 m/(mK) | 100 degre | 200 degre | 300 degre | 400 degre | 500 degre |
11.1 | 12.1 | 12.9 | 13.5 | 13.9 | |
Pwopriyete Fizik
Gwosè mm | Mwens pase oswa egal a 11 | 12-30 | 31-63 |
R Mpa | 1180-1420 | 1080-1320 | 980-1270 |
Rp 0.2 Mpa | Pi gran pase oswa egal a 835 | Pi gran pase oswa egal a 785 | Pi gran pase oswa egal a 685 |
Yon pousan | Pi gran pase oswa egal a 7 | Pi gran pase oswa egal a 8 | Pi gran pase oswa egal a 5 |
C pousan | Pi gran pase oswa egal a 30 | Pi gran pase oswa egal a 35 | Pi gran pase oswa egal a 35 |
Kv J | Pi gran pase oswa egal a 44 | Pi gran pase oswa egal a 44 | |
Dite HB | 354-406 | 327-384 | 295-373 |
Pwopriyete mekanik
Fòje
DIN 1.6587|17CrNiMo6 |18CrNiMo7-6 Forge tanperati: 900 - 1100 degre, fre dousman nan sab la apre fòje.
Tretman Chalè
Nòmalize: 850 - 880 degre / lè
Recuit mou: 650 - 700 degre / gwo founo dife
Soulaje estrès:630- 650oC
Carburising: 880 - 980 degre
Nwayo redi: 830 - 870 degre / dlo
Recuit entèmedyè: 630 - 650 degre
Ka redi: 780 - 820 degre / dlo
Tanperaman: 150-200 degre
Sifas dite
Trete pou amelyore kapasite pou tande (plis S): Max 255HB
Mou rkwit (plis A): Max 229HB
Trete nan ranje dite (plis TH): 179-229HB
Trete ak estrikti ferit-perlit ak ranje dite (plis FP): 159-207HB
Aplikasyon
DIN 1.6587|17CrNiMo6 |18CrNiMo7-6 asye pou pati ki mande fòs rupture nwayo ak dite segondè. Sanssib a gwo pati yo te sezi ak gwo rezistans mete ak chaj tankou: kousin lou ak BEARINGS, disip Cam, chen anbreyaj, boulon COMPRESSOR, ekstrè, Arbr fanatik, angrenaj lou, Arbr ponp, piyon, Tappets, mete broch, fil. Gid elatriye.



Anbalaj & Shipping
Tan livrezon: Livrezon se 7-15jou apre konfimasyon lòd acha ak peman davans.
Anbalaj: Creole pakè ekspòtasyon maritim, oswa jan sa nesesè.

Baj popilè: 18crnimo7-6 ba asye alyaj
Ou ka renmen tou